DONCASTERS SUPERALLOYS OF LONG BEACH
Doncasters Superalloys of Long Beach (Certified Alloy Products Inc.) specialises in the production of high-performance vacuum-refined superalloys for use in aerospace and industrial gas turbine engines, as well as other demanding commercial and industrial applications.
Using advanced technologies, our process expertise, extensive product offering and metallurgical know-how serves a global customer base. As a result, our facility maintains a variety of OEM, industry and quality related accreditations to produce master melt superalloys from various blended elements including nickel, cobalt, chrome, molybdenum, rhenium, hafnium, tungsten, tantalum and other alloying elements.
- Nickel and cobalt based alloys for equiax, directionally solidified (DS), single crystal (SX) and powder applications
- Billet weight: 20 to 550 lbs. (9 – 250kgs), and 15-lb. air melt pigs
- Ingot diameters from 1.625 – 7 in (41 – 178mm) – as well as notch and break cut to weight
- 100 different alloy types from Iron to Cobalt to Nickel based
- Vacuum melt from 550 – 22,000 lbs (250 – 10,000kg)
- Air melt up to 3,200 lbs (1,450 kg)
- Specialty R&D melts ~ 350 lbs (159 kg)
- Revert processing
- Wire EDM and ingot grinding
Vacuum melt up to
(10,000kg)
Air melt up to
(1450kg)
Accreditations:
- AS9100 Rev D
- ISO9001:2015
- NADCAP
Approvals:
- Space OEMs